                                                       ALT EGA X 100
                           Concentrate dispersion and egalize material
PRODUCTION SPECIFICATION

Chemical Composition : Combination of suitable non-ionic ether and esters
Ionic Character : Non-ionic
Appearence : Light yellow clear,voscous liquid
Ph : 6-7

PROPERTIES :

*ALT EGA X 100 is a perfec disperse and egalize material
* It is foam regulated.
* It is supply uniform leveling dispers dye in poliester dyeing İndantren and reactive dye in cottons dyeing ,kationic dye goups in acrilic dyeing, acid,crom and metal complex dyes inwool dyeing baths.
* It is prevent aglomeration and waste on dying equipment
* It is proved perfect smooh dyeing handle.
* It is prevent formation of oligomer.
* Its high stability dispers and egalize metaril so,it is perfect work in high temperature and high pressure for dyeing poliester and their mixtures.
* There is needlessness washing process after dyeing because of prevent formation of oligomer.
* It is mix with water in all ratio.
* It is used with non-ionic,anionic and cationic dyes , auxiliary chemicals ,acids,salt etc.
* It is used with all kind of carrier.
* It is used for dyeing knitting ,weawing fabrics,bobbib,carpet and fibres dyeing.

APPLICATION

* The bath temperature is adjuct to 50-60 C
* The ph value is regulate 4.5-5
* Add in dyeing bath 0.3-0.6 g/lt ALT EGA X 100. İf need you can a add other auxiliary chemicals in bath .
* Operate the machine 5 minutes before adding dyestuff.
* Add the dyestuff which is filtered than work the machine .10-15 min İn 50-60 C bath temperature.
* Increase the bath temperature to 130 C by the 1-1,5 C/min.
* Work the machine in this 130 C temperature between 60-90 min.according to colour of light or deep.
* Reduce the bath temperature slowly to 70-80 C after finishing dyeing and than drain the water .if need make reductive washing
• Generally there is no need final cleaning operation dyeing with ALT EGA X 100. For the correction of the poliester goods dyeing with poliester dyes in condition of HT( high temperature ) 0.3-0.6 g/lt ALT EGA X 100 at 125-135 C work wachine 1 hour.and then apply below washing process.0.3-0.6 g/lt ALT EGA X 100 1.0-2.0 g/lt sodium hydrosülfite 3.0-5.0 g/lt sodium hydroxide (35 Be)
Temperature :70 C
Time : 10-15 min.

General usage is recomended below
For diepersant : 0.3-0.6 g/lt
For egalizator : 0.5-1.0 g/lt
Extraction of dye :1.0-2.0 g/lt

STORAGE LIFE : Original package and normal temperature 6 month
PACKAGING : 60 Kg plastic carboys and 120 kg plactic barrels
Warning : All above information is best of our knowledge obtained during process and research.Every user of
our products should verify the data under his own conditions.

 

Dispersing and leveling agents

 

Leveling agent of nylon
 

Crease preventative agents
 

Fixing agents


Carier


Printing pat


De-foaming agents


DISPERSING AND LEVELING AGENTS